Specification

What goes down.

Base150 mm MOT Type 3 open-graded stone, compacted
BinderUV-stable polyurethane, hand-trowelled
Aggregate3 to 6 mm graphite, silver or flint
Depth18 mm
DrainageFully permeable, SuDS compliant
Cure24 hours foot, 48 hours car
Good to know

Straight answers.

Will it go slippery in the wet?
No. The exposed aggregate gives it grip, and it is rated for domestic vehicles.

Can it go over my old tarmac?
Often, if the tarmac is sound. We check it first and tell you honestly.

How does it age?
It will lighten a shade over the first year. A yearly jet wash keeps it crisp.

01

Survey

Levels, edges and drainage.

02

Dig

Out to depth, edgings set.

03

Base

Open-graded stone, compacted.

04

Lay

Resin mixed, trowelled, done.